A.Blended Polyol 


ItemIndex
Material Temperature20~25℃
Mold Temperature45~60℃
Cream Time6~10s
Rising Time40~80s
Demold Time120~240s
POL/ ISO Ratio100:40~65


*The actual reactivity characteristics may be adjusted according to process conditions and clients’ requirements


B.ISO 


BrandNCO%Details
JHW859825.71Modified MDI, widely operation window
JHW852927.91Modified MDI, widely operation window
JHW853226.5Modified MDI, widely operation window
JHW880332Mixed Modified MDI,apply in PIP headrest, Good liquidity